Computational references are not experiments: pre-registered validation of machine-learned sodium-cathode voltages
원문 초록
Machine-learning screens for battery materials are trained and judged almost entirely against computed reference voltages, and those references carry their own systematic errors. We report a case in which this matters quantitatively: our own screening stack (a graph-network voltage screen, a prior-art triage layer, and a local PBE+U bench) fails pre-registered validation against experiment-anchored literature values. Verdict thresholds, failure modes, and the primary metric were committed before analysis. On an operator-audited set of known Na-ion cathodes (n = 6 after one documented exclusion; verdict unchanged at n = 7), the raw held-out mean absolute error was 0.67 V, the pre-registered conservative metric, the upper 95% confidence bound of the cross-validated bias-corrected error, was 1.09 V, and the residual was strongly voltage-dependent (r = -0.94), so no additive calibration is valid. On the two compounds where prediction, database reference, and experiment could all be compared, the Materials Project PBE+U reference sat about 0.54 V below measurement: the reference, not the model, dominated the error. A prior-art screen found at least 70% of the targeted Na substitution space already published. We retire the screen, bound what "verified" means for our DFT ledger, and pre-register a calibration audit of it against four benchmark Li couples.
제출 이력
확인된 버전만 표시합니다. 전체 제출 이력은 arXiv 원문에서 확인하세요.
- arXiv:2606.23725v1제출 시각 미확인
함께 살펴볼 논문
공통 태그를 근거로 연결했습니다. 실제 인용 관계나 논문의 우수성을 뜻하지 않습니다.
공통 태그로 연결된 공개 논문이 아직 없습니다.
토론
이 논문과 연결된 포럼 글이 아직 없습니다.